Proficiency Test Study on Differential Scanning Calorimetry (DSC) Analysis of Plastics

Share this News

It is planned to organize the following proficiency test studies in the field of "DSC-Differential scanning calorimetry" taking into account the need in our country in order to evaluate the technical competence of accredited test laboratories in the field of "thermal analysis methods in materials".

1. DSC Analysis: Determination of melting point and enthalpy, ISO 11357-3 and ASTM D3418 (Thermoplastic)
2. DSC Analysis: Glass transition temperature, ISO 11357-2 and ASTM D3418 (Thermoplastic)

In September 2021, in order to participate in the proficiency tests to be held in September 2021, the "Interlaboratory Comparison / Proficiency Application Form", which can be accessed from the "Quick Access" section of our web page, must be filled in and submitted to ume@tubitak.gov.tr and  ume.yeterliliktesti@tubitak.gov.tr addresses for the application to be sent to.
 